| Thickness μm | 38 | 25 | 25 | 21.5 | 20 | 20 | 18 | 17 | 16 | 16 | 12 |
| JIS Gurley seconds | 780 | 620 | 515 | 320 | 530 | 560 | 500 | 450 | 435 | 460 | 425 |
| Porosity | 45% | 39% | 35% | 50% | 39% | 36% | 35% | 35% | 35% | 39% | 38% |
| PP Pore Size μm | 0.035 | 0.028 | 0.041 | 0.038 | 0.027 | 0.032 | 0.032 | 0.032 | 0.032 | 0.026 | 0.026 |
| TD Shrinkage @90°C/1hour | 0.0% | 0.0% | 0.0% | 0.0% | 0.0% | 0.0% | 0.0% | 0.0% | 0.0% | 0.0% | 0.0% |
| MD Shrinkage @90°C/1hour | <7.0% | <5.0% | <5.0% | <5.0% | <5.0% | <4.0% | <5.0% | <5.0% | <2.5% | <1.0% | <1.5% |
| Puncture Strength grams | >550 | >380 | >320 | >400 | >360 | >300 | >300 | >245 | >220 | >300 | >225 |
| TD Tensile Strength kgf/cm² | 165 | 150 | 170 | 140 | 165 | 185 | 175 | 190 | 180 | 150 | 155 |
| MD Tensile Strength kgf/cm² | 1630 | 1700 | 1680 | 2195 | 2050 | 1800 | 1800 | 1900 | 2085 | 2100 | 2200 |